Showing results 871 - 880 out of 942
1999
Wilke, M & Behrens, H 1999, 'The dependence of the partitioning of iron and europium between plagioclase and hydrous tonalitic melt on oxygen fugacity', Contributions to Mineralogy and Petrology, vol. 137, no. 1-2, pp. 102-114. https://doi.org/10.1007/s004100050585
Withers, AC, Zhang, Y & Behrens, H 1999, 'Reconciliation of experimental results on H2O speciation in rhyolitic glass using in-situ and quenching techniques', Earth and Planetary Science Letters, vol. 173, no. 3, pp. 343-349. https://doi.org/10.1016/S0012-821X(99)00228-9
Withers, AC & Behrens, H 1999, 'Temperature-induced changes in the NIR spectra of hydrous albitic and rhyolitic glasses between 300 and 100 K', Physics and chemistry of minerals, vol. 27, no. 2, pp. 119-132. https://doi.org/10.1007/s002690050248
1998
Becker, A, Holtz, F & Johannes, W 1998, 'Liquidus temperatures and phase compositions in the system Qz-Ab-Or at 5 kbar and very low water activities', Contributions to Mineralogy and Petrology, vol. 130, no. 3-4, pp. 213-224. https://doi.org/10.1007/s004100050361
Behrens, H & Schmidt, MO 1998, 'Infrared spectroscopy of hydrous silicic glasses at temperatures up to 600°C and implications for the incorporation and dynamics of water in glasses', Neues Jahrbuch fur Mineralogie, Abhandlungen, vol. 172, no. 2-3, pp. 203-226.
Fritze, H, Jojic, J, Witke, T, Rüscher, C, Weber, S, Scherrer, S, Weiß, R, Schultrich, B & Borchardt, G 1998, 'Mullite based oxidation protection for SiC-C/C composites in air at temperatures up to 1900 K', Journal of the European Ceramic Society, vol. 18, no. 16, pp. 2351-2364. https://doi.org/10.1016/S0955-2219(98)00242-8
Gesing, TM & Buhl, JC 1998, 'Crystal structure of a Carbonate-Nosean Na8[AlSiO4]6CO3', European journal of mineralogy, vol. 10, no. 1, pp. 71-77. https://doi.org/10.1127/ejm/10/1/0071
Hackbarth, K, Fechtelkord, M & Buhl, JC 1998, 'Crystallization kinetics of Na7.4(AlSiO4)6(CO3)4.7 4H2O, an intermediate phase between cancrinite and sodalite, grown under low temperature hydrothermal conditions', Reaction Kinetics and Catalysis Letters, vol. 65, no. 1, pp. 33-39. https://doi.org/10.1007/BF02475312
Ishihara, H, Horiuchi, K, Dou, SQ, Gesing, TM, Buhl, JC, Paulus, H & Fuess, H 1998, 'Isolated versus condensed anion structure IV: An NQR study and X-ray structure analysis of [H3N(CH2)3NH3]CdI4 · 2H2O, [H3CNH2(CH2)3NH 3]CdBr4, [(CH3)4N]2CdBr4, and [(CH3)3S]2CdBr4', Zeitschrift fur Naturforschung - Section A Journal of Physical Sciences, vol. 53, no. 8, pp. 717-724. https://doi.org/10.1515/zna-1998-0813
Pimenov, A, Ullrich, J, Lunkenheimer, P, Loidl, A & Rüscher, CH 1998, 'Ionic conductivity and relaxations in ZrO2-Y2O3 solid solutions', SOLID STATE IONICS, vol. 109, no. 1-2, pp. 111-118. https://doi.org/10.1016/s0167-2738(98)00082-4